A New Question for Sintering Masters: "Why Did It Crack?"

Articles · · Ali Parlar

A New Question for Sintering Masters: "Why Did It Crack?"

This time our job looks easier… The image shows a few cracked zirconia restorations, and we ask you:

“From the details in the picture, can you guess why these restorations cracked?”

The comments under the post were very rich and thought-provoking in terms of technical discussion.

🔍 Some Guesses:

  • “The program may be faulty; the heating is too fast and the holds are missing.”
  • “The outer parts took on colour but the bar stayed light, which indicates a different temperature distribution.”
  • “Zirconia does not conduct heat well; heating at different rates from the outside in may have caused the cracking.”
  • “This kind of cracking is usually caused by uneven heating, not by cooling.”
  • “The connector points may have been left too thin.”
  • “Upright positioning may have created a difference in contact with the insulation.”

Some attributed the cause of the cracking to the firing program, while others argued that it could stem from the positioning of the piece or from technical constraints.

💡 What About You?

What do you pay attention to during sintering? Upright or horizontal? How important are the hold steps, the exit rate, the ramp and the cooling?

To see the post with all these ideas and detailed comments: 👉 Visit our Instagram page and share your own comment!