Zirkonart Zirkon Blokları İçin Önerilen Pişim Programları

Suggested Firing Programs for Zirconart Zircon Blocks

Zirkonart


MP1500 tegra Speed ​​(4-step ovens)


Zirkonart up to 14 members

Step/Step temperature(C) Speed(C/min) Standby(min)
one
300
10 0
2 920 7.5 30
3 1460 3 120
4 300 9 30 (Lift Opening min)

 

Zirkonart up to 3 members

Step/Step
temperature(C) Speed(C/min) Standby(min)
one
300
10 0
2
1220
20 30
3
1460
8 60
4 300 15 30 (Lift Opening min)

 

Back to blog
  • Dişçilik için Zirkonya İşleme Süreci: Saflaştırılmış Sıvıdan Nihai Zirkon Blok

    Dental Zirconia Processing: From Purified Liqui...

    Introduction In the previous blog post, we explained the natural origin of zircon and how it is transformed into zirconium oxychloride, a purified liquid material. This liquid is the starting...

    Dental Zirconia Processing: From Purified Liqui...

    Introduction In the previous blog post, we explained the natural origin of zircon and how it is transformed into zirconium oxychloride, a purified liquid material. This liquid is the starting...

  • Diş Hekimliğinde Kullanılan Zirkonya’nın Kökeni ve Ham Madde Aşaması

    The Origin and Raw Material Stage of Zirconia f...

    (Reference image by Robert Matthew Lavinsky, Wikimedia Commons).Introduction Zirconia is widely used in modern dental restorations because of its strength, long-term durability, and natural appearance. But before it reaches dental laboratories,...

    The Origin and Raw Material Stage of Zirconia f...

    (Reference image by Robert Matthew Lavinsky, Wikimedia Commons).Introduction Zirconia is widely used in modern dental restorations because of its strength, long-term durability, and natural appearance. But before it reaches dental laboratories,...

  • Tegra MP1500 - MoSi2 ısıtma elemanı silica tabakası rejenerasyonu

    Regeneration of the silica layer of the MoSi2 h...

    SiO2 (silikon dioksit) yenilenmesi belirli bir sıcaklık aralığında etkili olur. Hem termodinamik açıdan, hem olumsuz etkilerden korunarak silisyum oksit tabakası yenilenmesi için en uygun sıcaklık 1300°C civarındadır.

    Regeneration of the silica layer of the MoSi2 h...

    SiO2 (silikon dioksit) yenilenmesi belirli bir sıcaklık aralığında etkili olur. Hem termodinamik açıdan, hem olumsuz etkilerden korunarak silisyum oksit tabakası yenilenmesi için en uygun sıcaklık 1300°C civarındadır.

1 of 3